Technical Product Bulletin FOOD AND DRUG APPLICATION EPOXY ADHESIVE PRODUCT
DESCRIPTION: AA-BOND FDA16 is a medium viscosity epoxy resin system
specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP
biological reactivity tests, in vivo and received Class VI approval. PRODUCT
PROPERTIES: APPEARANCE Amber MIX RATIO, BY WEIGHT 100:33 / Resin:Hardener BENEFITS Medium
viscosity low
permeability Good resistance Class VI
approved CURE TYPE Heat cure or Room temperature TYPICAL APPLICATIONS Bonding, laminating By manufacturers of catheters Hearing aids dental products Other biomedical instruments and devices Repair
applications by: - Manufacturers of food preparation. - Processing. - Packaging
equipment. UNCURED
PROPERTIES: VISCOSITY @
25 °C CPS 4,700 @Temperature
77°F, 25°C SPECIFIC GRAVITY, CURED 0.900 g/cc POT LIFE 25 min SOLID CONTENT 100% VOLATILE ORGANIC COMPOUNDS (VOC) CONTENT 0.15 g/l WATER ABSORPTION , AFTER 24 HR SATURATION, % 0.30 MECHANICAL PROPERTIES: LAP SHEAR STRENGTH (Alum to Alum) 2,100 24 hr @ 25°C 3300 4 hr @ 65°C HARDNESS, SHORE D 86 4 hrs @ 65°C 75 24 hrs @ 25°C CURE SCHEDULE: 1 – 4 hours @ 65°C 72 hours @ 25°C ELECTRICAL
PROPERTIES: VOLUME RESISTIVITY 1.20e+14 ohm-cm THERMAL
PROPERTIES: CTE, LINEAR 29.4 µin/in-°F @ 68 °F GLASS TRANSITION TEMP,TG 97.0 °C, 207 °F OPERATING TEMPERATURE -70 to 145 °C GENERAL INFORMATION: For safe handling information on this product, consult the Material Safety Data Sheet, (MSDS). HOW TO USE: 1) Carefully clean and dry all surfaces to be bonded. 2) Apply AA-bond FDA16 completely mixed adhesive to the prepared surfaces, and gently press these surfaces together. Contact pressure is adequate for strong, reliable bonds; however, maintain contact until adhesive is completely cured. 3) Some separation of components is common during shipping and storage. For this reason, it is recommended that the contents of the shipping container be thoroughly mixed prior to use. 4) Some ingredients in this formulation provided may crystallize when subjected to low temperature storage. A gentle warming cycle of 52°C for 30 minutes prior to mixing components may be necessary. Crystallized epoxy components do not react as well as liquid components and should be re-dissolved prior to use for best results. AVAILABILITY: This epoxy can be supplied in various different packages.
Froo www.froo.com | Froo Cross Sell, Free Cross Sell, Cross promote, eBay Marketing, eBay listing Apps, eBay Apps, eBay Application